May 27, 2025 Остави съобщение

Какво е K500?

Какво е K500?

 

 

K-500 alloy, commonly referred to as "K-MONEL", is a precipitation-hardenable nickel-copper alloy. It has corrosion resistance similar to 400 alloy, but with higher strength and hardness. The addition of aluminum and titanium to the nickel-copper matrix allows it to be subsequently heat treated to improve mechanical Свойства . k -500 сплав също има ниска магнитна пропускливост и остава немагнитна в широк температурен диапазон, включително под-нулеви температури .

Индустрии и приложения
K-500 alloy is commonly used in the marine, chemical processing, oil and gas, pulp and paper, pharmaceutical, food processing, and electronics industries. End uses for K-500 alloy include fasteners, springs, chains, pump and valve components, drill collars, scrapers, scrapers, agitator shafts, impellers, Сензори, електрически компоненти и други силно корозивни приложения, при които са необходими якост и твърдост .

What is K500?What is K500?

Корозионна устойчивост:
The corrosion resistance of K-500 alloy is similar to that of 400 alloy. However, in the age-hardened condition, K-500 alloy may experience stress corrosion cracking in certain environments. K-500 alloy is resistant to hydrogen sulfide and is suitable for sour gas environments, making it an ideal choice for oilfield applications. The low corrosion rate of K-500 alloy in seawater makes it an ideal choice for the marine industry. Pitting may occur in still or low-velocity seawater, but the pitting rate gradually slows after the initial attack.

Изработка и топлинна обработка:
K-500 alloy can be fabricated by standard commercial processes. Hot working of K-500 alloy should be performed at temperatures between 1600℃F and 2100℃F, but care should be taken to avoid prolonged immersion at higher temperatures. After hot working, the material should be water quenched at a temperature not less than 1450℃F. Cold forming in the annealed condition can also be performed using standard methods, but forming may require considerable force. K-500 alloy is easiest to machine in the annealed condition. Therefore, it is best practice to machine to oversize, then age harden, and finally machine to final size. Shrinkage may occur during aging, Така че позволяват размерени допустими отклонения от 0 . 0002 в/в преди стареене.

K-500 alloy is best welded using gas tungsten arc welding (GTAW). AWS A5.14 ERNiCu-7 filler metal is typically used for joining. Since this filler metal is not age hardenable, weldments using this filler metal will not achieve the strength of the parent Метал . за заваръчни заваръчни средства, където се изисква якост, може да се използва AWS 5.14 ernifecr -2 метален метал.

The alloy should be solution annealed before aging to dissolve microstructural phases that may have formed during previous processing. If the material is hot worked, the annealing temperature should be 1800℃F. If the material is cold worked, the annealing temperature should be 1900℃F. The dwell time at temperature should be minimized to avoid excessive grain growth. A water quench immediately following the solution anneal will avoid partial precipitation of the age-hardening constituents. For optimum properties, age hardening of annealed (soft) material should be performed as follows: Heat the material to between 1100℃F and 1125℃F for 16 hours, then furnace cool at a rate of 15℃F to 25℃F per hour until the material reaches 900℃F. Once the material reaches 900 градуса F, охлаждането може да продължи чрез охлаждане на пещта, охлаждане на въздуха или гасене .