Информация за размери и толеранси за кръгли пръти от сплав 601

Стандартни размери на Inconel 601 кръгла лента

Диаметър или
ширина
(mm)
Тегло на метър Секционна площ Периметър
  Квадрат
(кг)
Кръгъл
(кг)
Квадрат
(cm²)
Кръгъл
(cm²)
Квадрат
(cm)
Кръгъл
(cm)
5.0 0.20 0.15 0.25 0.20 2.0 1.57
5.5 0.24 0.19 0.30 0.24 2.2 1.78
6.0 0.28 0.22 0.36 0.28 2.4 1.88
7.0 0.38 0.30 0.49 0.38 2.8 2.20
8.0 0.50 0.39 0.64 0.50 3.2 2.51
9.0 0.64 0.50 0.81 0.64 3.6 2.83
10 0.73 0.63 1.00 0.79 4.0 3.14
11 0.95 0.75 1.21 0.95 4.4 3.46
12 1.13 0.89 1.44 1.13 4.8 3.77
14 1.54 1.21 1.96 1.54 5.6 4.40
16 2.01 1.58 2.56 2.01 6.4 5.03
18 2.54 2.00 3.24 2.54 7.2 5.65
20 3.14 2.47 4.00 3.14 8.0 6.28
22 3.80 2.98 4.84 3.80 8.8 6.91
25 4.91 3.85 6.25 4.91 10.0 7.85
28 6.15 4.83 7.84 6.16 11.2 8.80
32 8.04 6.31 10.24 8.04 12.8 10.05
36 10.17 7.99 12.96 10.18 14.4 11.31
40 12.56 9.86 16.00 12.57 16.0 12.57
45 15.90 12.49 20.25 15.90 18.0 14.14
50 19.62 15.41 25.00 19.64 20.0 15.71
56 24.62 19.34 31.36 24.63 22.4 17.59
63 31.16 24.47 36.69 31.17 25.2 19.79
71 39.57 31.08 50.41 39.59 28.4 22.31
80 50.24 39.46 64.00 50.27 32.0 25.13

 

Inconel UNS N06601 Толерантност на ярки кръгли пръти

Inconel 601 Round Bar Толеранс ISO "H" серия в MM
Размер (mm) H12 H11 H10 H9 H8 H7 H6 H5
Над 180 - 250 +0.46/0 +0.29/0 +0.185/0 +0.115/0 +0.072/0 +0.046/0 +0.029/0 +0.02/0
Над 120 - 180 +0.4/0 +0.25/0 +0.16/0 +0.1/0 +0.063/0 +0.04/0 +0.025/0 +0.018/0
Над 80 - 120 +0.35/0 +0.22/0 +0.14/0 +0.087/0 +0.054/0 +0.035/0 +0.022/0 +0.015/0
Над 50 - 80 +0.3/0 +0.19/0 +0.12/0 +0.074/0 +0.046/0 +0.03/0 +0.019/0 +0.013/0
Над 30 - 50 +0.25/0 +0.16/0 +0.1/0 +0.062/0 +0.039/0 +0.025/0 +0.016/0 +0.011/0
Над 18 - 30 +0.21/0 +0.13/0 +0.084/0 +0.052/0 +0.033/0 +0.021/0 +0.013/0 +0.009/0
Над 10 - 18 +0.18/0 +0.11/0 +0.07/0 +0.043/0 +0.027/0 +0.018/0 +0.011/0 +0.008/0
Над 6 - 10 +0.15/0 +0.09/0 +0.058/0 +0.036/0 +0.022/0 +0.015/0 +0.009/0 +0.006/0
Над 3 - 6 +0.12/0 +0.075/0 +0.048/0 +0.03/0 +0.018/0 +0.012/0 +0.008/0 +0.005/0
~ до 3 +0.1/0 +0.06/0 +0.04/0 +0.025/0 +0.014/0 +0.01/0 +0.006/0 +0.004/0

 